Modern batteries, unlike older, are not subject to such global repair as a replacement of plates, etc. In some models, there is no possibility even to add water, not to mention something else. I will tell you what can be done if, as a result of an accident or for some other reasons, a crack appeared in the battery. I will say right away if the entire electrolyte of the output and the battery stood over the month, then most likely it can be thrown out due to the wave on the plates. To top up the electrolyte to the old one cannot, it will most likely bear the battery. Almost all corps rechargeable batteries Made of such plastic as\u003e PE< полиэтилен. Цитата из википедии: “ полиэтилен при комнатной температуре нерастворим и не набухает ни в одном из известных растворителей”. Если интересно, можете набрать в поисковике “ чем склеить полиэтилен “ и вы поймёте, что любой клей отпадает сразу. Технологии, конечно, не стоят на месте, может, что и придумают. Наплавить трещину обычным паяльником тоже не получится, в итоге всё равно потечет. Единственный, на мой взгляд, способ ремонта это сварка. Донора можно взять к примеру с бачка омывателя или подкрылка с маркировкой PE (БАМПЕР НЕ ПОДОЙДЁТ!). Ниже будет видео такого ремонта. При попытке набить клемму корпус лопнул. Как будет видно, хозяин аккумулятора сначала пытался трещину наплавить, потом заклеить. Концовка видео, почему то обрезалась, но я думаю, суть будет ясна.

Perhaps the most frequent breakdown, with which I had to face for 14 years of work, this is a crack on the neck of the butter. And the reasons for its occurrence are several. The first reason is poor-quality, eye or just immature wood. Unfortunately, in the conditions of mass production of weapons, the problem of selection good material Do not at all. The move seems to go all that fell under the saw. The second reason is the backlash between the shoe and the butt itself. I contributes to this as a poor-quality cutting of the mechanism and the weakening of the fastening of the gate group. On the guns with a central tie screw, given its greater length, the natural shrinkage of wood in 3-5% gives a very tangible gap between the metal of the pad and butt. Yes, and the carving can reach. In the guns with a wedge stop (for example, IL 54 or TOS), the butt is now manufactured at all without taking into account this emphasis. And the block holds simply on a pair of vertical screws supplied into the holes in wood with an intentionally increased diameter. Probably for the convenience of assembly. Breaks such buttons very quickly. And the third reason is pure "household injuries" somehow: drop from a quad bike or snowmobile, squirrels through a roof in a car, riding on jeep on guns, use instead of oars on a rubber boat, finishing pranks, or just clarifying relationships in a hand-to-hand attack. In short, a lot of reasons. That is the next beautiful beauty - a crack. This is the result of the "battle" with a flex in the Kostroma spill. (Photo number 1).
The first rule - the crack one does not "go." She necessarily has a sister and probably not even alone. And if they are not visible, then this is a matter of time or dirt along with impregnation. The rule is the second - no metal when repairing (screws, screws, ties, etc.). When we are at one time, the manufacture of billiard Kiyov, I firmly learned that it was impossible to glue the metal and a tree - it is impossible! Of course, this applies to adhesive connections experiencing shock loads. Foreign on its physico-mechanical properties The wood body will braid. And everything screwed or incurred screws will be internal stress concentrators and if they do not fly out, they will lead to the formation of new cracks around themselves. Also concerns all the screeds between the side cheeks. For some time there are enough of them, but then the butt comes in complete disrepair. I often bring the fruits of such "repairs" produced by fathers or grandfathers. And as a result, heirs already have to redo the whole butt.

The tree can be reinforced, in this case, only with a tree or bamboo. It is clear that the crack must be stuck so that it is no longer remembered. That is, ensure maximum strength in the adhesive connection. Everywhere you read: "Before gluing thoroughly degrease the glued surfaces." But how to provide inside the crack? Yes, in the trees impregnated with oils.

Output one: get rid of all impregnations, oils and dirt immediately in the whole butt, so I soak it entirely in solvents. For this, even suitable sizes of a wooden box (Photo No. 2),
covered with dense polyethylene. But necessarily tightly closed. Couple! You understand. In order to pull the most solar oils, I fill for the beginning of the White Spirit. Two liters should be enough. The main thing that he does not smell gasoline. After 2-3 days, if the solvent was very darkened, I change it on the fresh (depends on the degree of pollution of the tree and sometimes the process is delayed for a couple of weeks). Then I put the butt vertically on the nerve for drying. After about a day, immersing it in the same box, but already filled with pure acetone. It should be remembered that good quality acetone, suitable for this, dries on his hands without leaving odor. In it, I am withstanding two days. And I put it again vertically for final drying. A day later, two I get a clean tree, suitable for further gluing (photo No. 3).

It is possible to immediately soak in acetone, but only if the butt has a surface protective coating. In the event that oil penetrated deep into wood, excess osmotic pressure can lead to cracking material. After such processing, even those cracks that were not noticeable are opening (remember about sisters?). (Photo number 5)
In order to fill the cracks with glue (in this case, it is two component resin) I "reveal" the brushes. That is, I impose a clay on the neck of the clamp of the clamp, in order to avoid further crack growth, and slowly squeezing the brushes with the help of a wooden wedge. At the same time, the slot is smoothly so much so that it is possible to get the ability to penetrate the crack with a sharpened bamboo stick or a kapron thread. With the help of which filling the cavities of the resin. (Photo number 4) Next, removing the wedge and clamp, tightening the place of the gluing the elastic medical bandage. It allows you to evenly enhance gluing throughout the area, not deforming the notch. And besides, it does not stick to the resin. (Photo number 6)
It should be borne in mind that each round multiplies the squeezing effort. With excessive tightening, all glue may be extruded and "hungry" gluing will occur. And this means hopelessly spoiled butt. Before working the resin, it is better to immediately toned in the desired shade to get an almost imperceptible place of gluing. For this purpose, I use pigments from tinting machines. Remnants that, in plastic bottlesAfter refueling the machine usually throw out, and it is required quite a bit. These pigments can be quite successfully mixed by achieving the desired shade. (Photo number 7)
The fracture gluing itself is not enough, especially if the wood is already "tired". Therefore, I am enhancering the neck of the bamboo spokes. I used to dismiss the father's bamboo fishing rods for this. Now they make chinese toothpicks. Their diameter is about 2mm, which is quite enough. First, place the installation locations of the spokes and gently set the channels with a drill, pulled to the manner drills on a tree, i.e. With clearly speaking forward by centering edge. Channels do not necessarily do through, but it is desirable that the tip of the drill seems to see from the opposite side. The tiny hole will help exit glue over the adjacent knitting needles. And sometimes you have to install the needles only with inner But how to spoil appearance Butt. The most important thing is to try to put the knitting needles under different angles, crossing possible directions for the formation of cracks. (Photo number 8) Even by itself, the "firmware" by the spokes in mutually intersecting directions is largely enhanced by the neck. Once, for the sake of the experiment, I "sewed" falling off with a decent part of the neck, a cheek without glue, only at 13 spokes. And this turned out to be enough so that the IZH 27 sustain two shots from both trunks without any consequences. On the second shot, we did not argue, but I am sure that the butt would stand it. That's actually all. It remains, after curing the resin, carefully cut the protruding parts of the knitting spokes, pass the place of gluing and impregnate with protective compositions. (Photo number 9)



Especially successfully mask the ends of the spokes when they fall in places with a notch. In the smooth areas you can slide the needles with the help of brown feltwasters. (Photo number 10). In the next article, I will tell you how to make a good notch with the easiest and most affordable tools. Sincerely, your bass

IN modern world It is difficult to imagine life without toilet bowl, a drain tank and other plumbing facilities. Of course, you need timely care. But, like everything in the world, plumbing can also sometimes break out, and then you have to repair it. Do not wait for your toilet to fall apart.

Concept of drain tank.

As soon as the most insignificant malfunction appeared, crack, do not postpone the repair, but begin to act.

Then your bathroom will last very long and in good condition.

If the toilet cracked

Repair of the toilet, at first glance, may seem difficult, so many just cause a master who will do everything, but will definitely take some amount of money with you. Perhaps it seems to be the only way out, especially if you have never come across such problems before. Yes, and many simply do not know what you can take the toilet. But you should not make hasty conclusions. Try to eliminate the breakdown yourself, especially if the problem is that your toilet or tank cracked. After all, the crack can be stuck. The main thing is not to panic and do work carefully.

So, if you encountered the fact that your toilet gave a crack, then you must first find out exactly where there was a breakdown. And it is not at all necessary to consider how much money left in your wallet and remember where there is a store with plumbing nearby, because you can fix this problem yourself with the help of remedies. Consider the moments when you have a crack on the toilet, a drain tank or if a piece of ceramics from them broke off. All this is fixable if you come to this case correctly.

Drawing toilet bowl.

If there is a crack on your toilet, then it must be stuck as soon as possible. Firstly, so that it does not get even more, and secondly, so that water does not succe. To make a crack that was formed on the toilet, it is necessary to have glue. It should be waterproof. You can also use cold welding or silicone sealant. Find sandpaper and spatula. Well, if you also have construction Fen.

When you found everything you need for repair, you can directly to it and start. Take the construction hairdryer and warm the crack. It must be done not only outside, but also inside. Such actions are necessary in order to excess moisture evaporated. It is necessary to degrease the surface on both sides. To do this, use either acetone or solvents. Next, carefully lubricate the surface with epoxy resin. Then make the plastic strips on both sides and wait until everything is dry. And at the very end, the waterproof glue should be applied to the crack.

But it happens that a piece of ceramics simply broke from the toilet. Then you need glue that should be waterproof. Apply the glue on a thin layer on a breakaway piece, press it to the place from which it broke out, and after four hours it will stick. Next, treat that seam that has been formed from you, for seams or epoxy resin with filler. After that, it is better to clean the place of sandpaper.

Solving problems with drain tank

If the problem is that you cracked exactly cistern, then you need to determine where the crack is. Usually they appear on the walls of the toilet bowl. This is due to the fact that mechanical impacts occur on the walls most often. Deciding to repair the tank, it is necessary to take care that the water is blocked, and there was no water inside it. Next, it is necessary to carefully open the cover of the tank (because if you break it, it is unlikely to be able to find the same) and completely dry it. And only after these actions can handle the crack with the help of sealant and wait until it dries.

Now you need to try the drain tank. To do this, try to get water into it and wait until the tank is complete. And after that, you can watch whether it proceeds or your efforts did not pass in vain. But, if nevertheless, after your actions, the tank flows, then in this case it will have to change it. This happens rarely, basically, it can be repaired independently, even if he cracked.

Plastic buckets, cans and tanks - things on cottage plot Necessary. Often, in the conditions of the cottage, there is no possibility to change the old burst plastic container for a new product, but, if desired, it can always be repaired. About how it can be done is described below.

If the plastic bucket bursts the bottom, then it is useless to try to stick it. No glue will endure a long pressure poured into the container of the liquid and over time the crack on the plastic will necessarily disappear.

It can be much more reliable to repair the broken bucket, throwing the crack in it with another suitable piece of plastics.

To do this, you will need:
large and powerful soldering iron;
Plastic tape, which, for example, can be cut from an unnecessary PET bottle, or plastic chomoth;
any detergent.


Tightening the crack is necessary both inside the bucket and outside, and, and it is recommended to start on the side of the inner, since there are crack edges that can be put on top of each other, resting them into the surface on which the bucket stands.


If you start working with outdoor Cracks, then its edges will spring, fall and impose them on each other tightly it will be difficult.


However, for the convenience of perception, we will look at, after all, as weave the crack on the plastic bucket on its side of the outside, bearing in mind that it is already closed inside the tank.

So, in order to pour a plastic bucket:
1. Its surface around the crack is thoroughly wash and degrease.


2. Include a soldering iron, wait for it and smooth movements to the right and left to water his sting along the crack, not pressing on the plastic so that it does not burn it. Thus, melting plastic on the edges of the crack, stealing the soldering iron along its entire length.


3. Sequentially laid plastic tape on a crack, starting from a point a little further than its start. In this case, the tape is heated by a soldering iron so that the melted plastic filled the cavity of the crack, that is, expressing figuratively, they are sealing.



4. After seating, the cracks are obtained by seam, which is additionally smoothed by a hot soldering iron, moving his sting along this peculiar "welded" line.


It is so easy and without special tricks that can be seized with a crack on a plastic bucket or any other made of plastic containers. Inside the bucket of the seam is performed on the same technology.


It remains only to check whether it does not occur after repair.

Video of the process of seating the crack on the plastic bucket:

It is not necessary to call the wizard or call a neighbor, you can independently and without special efforts Pack the cracked glass at home. This kind of repair will not spoil the appearance of the glass and is able to hold out about two or three years. Do not be afraid to wash the glass in the place of gluing, it is absolutely safe!

For this type of repair you will use silicone glue and brushes, syringe and acetone, a little detergent And transparent varnish. Grab the ordinary cloth for cleaning in the apartment and cotton swabs. Type the water in the bucket and do not forget to take a few acetone.
Preparation of cracked glass to repair

First of all, clean the windows and glass from dust and dirt. Rinse them with a solution of water with a detergent for glass. Divide the remedy in a bucket with warm water according to the proportion specified in the instructions on the detergent label. Wash the glass in rubber gloves. So you protect your hands from negative impact chemicals For washing glass.

Wash glasses are necessary on both sides. After washing dry, wipe them with a clean cloth. In place of cracks, be extremely careful not to cut down the glass. Now we are waiting for glasses to dry finally. See that there is no water in the cracker place, because in this case the glue will be bad.

After the glass dried, it is necessary to degrease the place of the crack. Take a cotton swab and wetting it in acetone. All work performed in rubber gloves! A glue will be applied much better for a degreasing surface and its layer will be even more careful. Moreover, in this case, the service life will significantly last. Much more convenient to process acetone with a cotton wand. See if the wool is not synthetic, then she can leave the cotton patches followed. In this case, it is more convenient to use gauze.
We rush the crack on the glass

We proceed directly to the cracking of the crack. To do this, take and type silicone glue into the syringe (without needle), make a crack carefully. It is necessary to do this slowly and confidently so that the glue can evenly distribute over the entire surface of the crack and damaged glass.

Some tubes of silicone glue have a facility with a comfortable tip that allows you to squeeze small portions of glue. If the crack on the glass is large, then after applying glue, glue it from both sides with a transparent scotch. Performed work leave 12 hours before complete drying.

On top of the cracks we apply a thin layer of transparent varnish. Take a thin brushing, carefully mock it in varnish and spend on the place of gluing. It remains to wait for a lacquer drying and everything is ready!